代表性文章 | [1] Yang Y*, Qian H. Investigation on Aging σ-Phase Precipitation Kinetics and Pitting Corrosion of 22 Pct Cr Economical Duplex Stainless Steel with Mn Addition[J]. Metallurgical and Materials Transactions A, 2018, 49 (8): 3184-3197 [2] Yang Y*, Cao J, Gu Y. Investigation on the solution treated behavior of economical 19Cr duplex stainless steels by Mn addition[J]. Materials & Design, 2015, 83: 820-828. [3] Feng Z, Yang Y*, Wang J. Effect of Mn addition on the precipitation and corrosion behaviour of 22% Cr economical duplex stainless steel after isothermal aging at 800° C [J]. Journal of Alloys and Compounds, 2017, 699: 334-344. [4] Yang Y*, Yan B. Effect of high temperature compression deformation strain rate on the microstructure and corrosion behavior of 2205 duplex stainless steel[J]. Anti-Corrosion Methods and Materials, 2015, 62(3): 163-171. [5] Yang Y*, Yan B. The microstructure and flow behavior of 2205 duplex stainless steels during high temperature compression deformation[J]. Materials Science and Engineering: A, 2013,579:194-201. [6] Yang Y*, Yan B, Li J, et al. The effect of large heat input on the microstructure and corrosion behaviour of simulated heat affected zone in 2205 duplex stainless steel[J]. Corrosion Science, 2011, 53(11):3756-3763. [7] Yang, Y. H, Yan, B, Wang, J, et al. The influence of solution treatment temperature on microstructure and corrosion behavior of high temperature ageing in 25% Cr duplex stainless steel[J]. Journal of Alloys and Compounds, 2011, 509(36): 8870-8879. [8] Yinhui Yang, Biao Yan, Junlin Yin, et al. Microstructure and corrosion behaviour aging at 750 °C in 25% Cr duplex stainless steel[J]. Rare Metals, 2011, 30(1): 515-519. [9] 苏煜森, 杨银辉*, 曹建春等. 节 Ni 型 2101 双相不锈钢的高温热加工行为研究[J]. 金属学报, 2018, 54(4): 485-493. [10] 杨银辉*, 柴锋, 严彪等. Ti处理改善船体钢焊接粗晶区的低温韧性研究[J]. 金属学报, 2010, 46(1): 62-70. [11] 白于良, 杨银辉*, 曹建春, 等. Mn 对 22% Cr 双相不锈钢 700℃ 时效 σ 相及韧性的影响[J]. 材料工程, 2017, 45(5): 71-79. |